For reducing the cost of steel making!! Sharp decrease in Electrode consumption with simple coating method!!! High performance antioxidant for Graphite Electrode!!!!
Natural impregnating method
This is the simplest method and most suitable when the number of electrodes to be impregnated are relatively few.It uses an ordinary steel tub of which the inside has been coated with acid-resistant paint and economizes initial cost for user.Impregnating time, which varies with electrode quality, is almost 10 to 30 minutes.

Stock Yard of Electrode
Impregnating (1) Impregnating (2)
Click above picture and you can get the enlarged picture!!